- 출판일1995.07
- 저자
- 서지사항
- 등록일
2016.11.02
- 조회수
231
The method comprises feeding a first yarn at a first rate to an air-texturing jet and simultaneously feeding a second yarn at a second rate to the air-texturing jet to form a composite yarn. The composite yarn is withdrawn from the air texturing jet at a third rate which is lower than the first two rates whilst periodically reducing the second rate by increasing the yarn path of the second yarn and allowing the increased yarn path to suddenly return to the original yarn path to form slubs in the composite yarn in the air-texturing jet. The yarn is then fed to an air commingling jet. IPC D02G.